ERNiCrMo-4/UNS N10276/W. Nr. 2.4819 AWS A5.14 Wire

PRODUCT PARAMETERS

Overview


ERNiCrMo-4 is a nickel-based superalloy with nickel, chromium, molybdenum and other elements as its main components. Among them, nickel is the main element in the alloy, which can improve the corrosion resistance and high temperature strength of the alloy. Chromium can improve the oxidation resistance and corrosion resistance of the alloy. Molybdenum element can improve the high temperature strength and toughness of the alloy. In addition, ERNiCrMo-4 also contains a certain amount of iron, cobalt and other elements to adjust the mechanical properties and processing properties of the alloy.

ERNiCrMo-4 Nickel Alloy C276 is used for welding materials of similar chemical composition as well as dissimilar materials of nickel base alloys, steels and stainless steels.  This alloy can also be used for cladding steel with nickel-chrome-molybdenum weld metal. 



ERNiCrMo-4 (Weldme 276) have an excellent corrosion resistance in a wide range of severe environments. The high molybdenum content makes the alloy especially resistant to pitting and crevice corrosion. The low carbon content minimizes carbide precipitation during welding to maintain corrosion resistance in as-welded structures.


Limiting Chemical Composition, %


Nickel..................................................................................................................................................................................51.23-63.50

Chromium...........................................................................................................................................................................14.50-16.50

Molybdenum......................................................................................................................................................................15.00-17.00

Iron..........................................................................................................................................................................................4.00-7.00

Tungsten.................................................................................................................................................................................3.00-4.50

Cobalt......................................................................................................................................................................................2.50 max.

Manganese.............................................................................................................................................................................1.00 max.

Carbon.....................................................................................................................................................................................0.01 max.

Vanadium................................................................................................................................................................................0.35 max.

Phosphorous.......................................................................................................................................................................... 0.04 max.

Silicon......................................................................................................................................................................................0.08 max.

Sulfur........................................................................................................................................................................................0.03 max.



Physical Constants


Density

g/cm^3............................................................................................8.89

Melting Range

°F .........................................................................................2417-2498

°C .........................................................................................1325-1370

Thermal Conductivity

at 20°C (68°F).................................................................................116



Tensile Properties


Tensile strength Rm (MPa)

Elongation A %

Temperature(°C)

> 724

≥40

+20



Corrosion Resistance


ERNiCrMo-4 has excellent corrosion resistance and can resist the role of corrosive media such as atmosphere, seawater, acid and alkali. At high temperatures, the chromium element in the alloy can form a dense oxide film, which further enhances its corrosion resistance.

Product Forms And Packaging (0ther sizes available -please contact us)



Product



Diameter



Length



Packaging



Wire For MIG/GMAW Welding



0.8mm/1.0mm/1.2mm/1.6mm/2.0mm/2.4mm /2.5mm/3.2mm



-



33 lbs (15kgs)



Rods For TIG/GTAW Welding



2.0mm /2.4mm /2.5mm/3.2mm/4.0mm/5.0mm



915mm-1000mm



11 lbs (5kgs)



Wire For SAW Welding



2.0mm /2.4mm /2.5mm /3.2mm /4.0mm/5.0mm



-



60 lbs (27kgs)


FAQ

Q1. What is your terms of Packing?

A: Generally we pack your goods with Neutral English bag, PP Woven bag with PE inner bag. If you have your own legally registered sack design, we can pack your goods with your brand and design bags after getting your authorization letter.

Q2. What is your terms of payment?

A: Normally 30% TT as deposit in advance, and 70% TT after email the copy of BL. Or LC at sight. We'll show you the photos pf your goods and package before you arrange the payment.

Q3. What is your terms of delivery?

A: Normally we do FOB, CFR, CIF terms.

Q4. How about your delivery date?

A: Normally it will takes 10~15 days after receive the deposit. The specific delivery time depends on the items and the quantity of the order.

Q5. Can you produce according to the sample?

A: Yes, we can produce by your samples or the specification you provide.

CONTACT US

PRODUCT RECOMMENDATION